ROUGHNESS OF 1.0721 STEEL AFTER CORROSION TESTS IN 20% NaCl
PRODUCTION ENGINEERING ARCHIVES 15(2017), pp. 27-30
DOI: 10.30657/pea.2017.15.07

Abstract
Non-alloy quality case-hardening steels are used for low-load components made on automatic machining centers (automatic lines). Because of the widespread use of these steel in open constructions, they are exposed to atmospheric corrosion. The study attempted to analyze the effect of 20% aqueous NaCl solution on the roughness of the steel as a result of corrosion. The steel roughness and corrosion wear
were determined according to corrosion time.



Keywords
steel
corrosion
corrosion rare
roughness
NaCl solution